Additional Photos:
|
 |
 |
 |
 |
When fired at 1,650° for two hours, PMC3™ is the
strongest fine silver metal clay available. It has a finer, smoother
composition that’s easy to work with and manipulate. You can also embed
findings with confidence--firing at a low temperature means they won’t
be heat-damaged. PMC3 is suitable for torch-firing as well as
kiln-firing.
Composition: Metal powder (90%), water and organic binder (10%) Shrinkage: 12% Color: Pickle white Physical Properties: •
Firing temp.: 1,650°F (900°C) for two hours to achieve highest hardness
and maximum durability; or 1,110°F (600°C) for 45 minutes; or 1,200°F
(650°C) for 20 minutes; or 1,290°F (700°C) for 10 minutes. • Melting point: 1,762°F (960°C) • Density after firing: 9.3 specific gravity (rolled silver = 10.5 specific gravity)
|
|
 |
 |
 |
 |
|
|